Cyclic thermo-mechanical material modelling and testing of 316 stainless steel
(Elsevier ScienceDirect, 2010-04-20)A programme of cyclic mechanical testing of a 316 stainless steel, at temperatures of up to 600 C under isothermal conditions, for the identification of material constitutive constants, has been carried out using a ...