• Login
    ARAN - Access to Research at NUI Galway
    Search 
    •   ARAN Home
    • College of Engineering and Informatics
    • Search
    •   ARAN Home
    • College of Engineering and Informatics
    • Search
    JavaScript is disabled for your browser. Some features of this site may not work without it.

    Browse

    All of ARANCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsTypesThis CommunityBy Issue DateAuthorsTitlesSubjectsTypes

    My Account

    LoginRegister

    Statistics

    Most Popular ItemsStatistics by CountryMost Popular Authors

    Help

    How to submit and FAQs

    Discover

    AuthorLeen, Sean B. (1)Subject316 Stainless steel (1)Chaboche unified viscoplasticity model (1)Creep (1)
    Nickel-based superalloy (1)
    Plasticity (1)... View MoreDate Issued2010 (1)Type
    Article (1)

    Search

    Show Advanced FiltersHide Advanced Filters

    Filters

    Use filters to refine the search results.

    Now showing items 1-1 of 1

    • Sort Options:
    • Relevance
    • Title Asc
    • Title Desc
    • Issue Date Asc
    • Issue Date Desc
    • Results Per Page:
    • 5
    • 10
    • 20
    • 40
    • 60
    • 80
    • 100
    Thumbnail

    Cyclic thermo-mechanical material modelling and testing of 316 stainless steel 

    Leen, Sean B. (Elsevier ScienceDirect, 2010-04-20)
    A programme of cyclic mechanical testing of a 316 stainless steel, at temperatures of up to 600 C under isothermal conditions, for the identification of material constitutive constants, has been carried out using a ...